Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 61.0 µm/m-°C @Temperature -30.0 - 100 °C |
33.9 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hifaxâ„¢ Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB252 medium high melt flow, 1,200 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has very well balanced processability, rigidi.. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
33.9 µin/in-°F @Temperature -22.0 - 176 °F |
Borealis Method |
Borealis Daplen™ EE108U Polypropylene TPO Compound Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives.. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature 40.0 - 130 °C |
33.9 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 7500 Phenolic, Granular, Compression Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Cast 3011 Semi-Flexible Clear Epoxy Casting Compound TRA-CAST 3011 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life.. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Cast F311 Optically Transparent Semi-Flexible Casting System TRA-CAST F311 is a clear, low viscosity epoxy formulation developed for molding, embedding, casting and potting applications where clarity, toughness, long pot-life and superior impact properties ar.. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Cast FS255 Flexible Clear Epoxy Casting Compound TRA-CAST FS-255 is a clear, low viscosity, epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties -- good clarity, long pot.. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
|
Trelleborg Emerson & Cuming Stycast® 2072 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
|
Trelleborg Emerson & Cuming Stycast® 2651-40/23LV Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
CTE, linear | 61.0 µm/m-°C | 33.9 µin/in-°F | ASTM D696 |
Unitika U-100 Engineering Plastic CAS No: 26590-50-1Information provided by Unitika Ltd. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Devcon Combo Wear FC Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
CTE, linear | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Devcon Wear Guard (Fine Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
CTE, linear | 61.0 µm/m-°C | 33.9 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® 301-2 Optically Transparent Epoxy Product Description: EPO-TEK® 301-2 is a two component optical, medical, and semiconductor grade epoxy resin, with low viscosity, long pot-life, and good handling characteristics.Advantages & Appli.. |
|||
CTE, linear | 61.0 µm/m-°C | 33.9 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® 730 Unfilled Black General and Structural Grade Epoxy Material Description: A two component, room temperature curing, general and structural grade epoxy. It can be used for adhesive, sealing, and encapsulating applications in medical, xray device, fil.. |
|||
CTE, linear | 61.0 µm/m-°C | 33.9 µin/in-°F | 90 Minute UV Cure; T<Tg; ASTM E831-93 |
3D Systems Accura® SI 40 Plastic for the SLA® 250 System Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |
|||
CTE, linear | 61.0 - 104 µm/m-°C | 33.9 - 57.8 µin/in-°F | Average value: 74.0 µm/m-°C Grade Count:8 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
CTE, linear | 61.0 - 61.0 µm/m-°C @Temperature 60.0 - 138 °C |
33.9 - 33.9 µin/in-°F @Temperature 140 - 280 °F |
Average value: 61.0 µm/m-°C Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |