Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 80.0 - 90.0 µm/m-°C @Temperature 20.0 °C |
44.4 - 50.0 µin/in-°F @Temperature 68.0 °F |
DN.53752 |
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high.. |
|||
CTE, linear | 80.0 - 90.0 µm/m-°C @Temperature 20.0 °C |
44.4 - 50.0 µin/in-°F @Temperature 68.0 °F |
DN.53752 |
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high.. |
|||
CTE, linear | 80.0 - 90.0 µm/m-°C @Temperature 20.0 °C |
44.4 - 50.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
CTE, linear | 70.0 - 90.0 µm/m-°C | 38.9 - 50.0 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CQX10030E10 F Polypropylene, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
CTE, linear | 70.0 - 90.0 µm/m-°C | 38.9 - 50.0 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CQX10030E10 Polypropylene, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
CTE, linear | 70.0 - 90.0 µm/m-°C | 38.9 - 50.0 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CQX30030 RTX Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
CTE, linear | 70.0 - 90.0 µm/m-°C | 38.9 - 50.0 µin/in-°F | Polykemi |
Polykemi AB POLYfill PPC TS20020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 70.0 - 90.0 µm/m-°C | 38.9 - 50.0 µin/in-°F | Polykemi |
Polykemi AB POLYfill PPC TS20020 UV Polypropylene Copolymer, Mineral Reinforced, UV-Stabilized Information provided by Polykemi AB |
|||
CTE, linear | 80.0 - 90.0 µm/m-°C @Temperature 20.0 °C |
44.4 - 50.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C | 27.8 - 50.0 µin/in-°F | Average value: 76.0 µm/m-°C Grade Count:25 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
CTE, linear | 72.0 - 90.0 µm/m-°C @Temperature 0.000 - 156 °C |
40.0 - 50.0 µin/in-°F @Temperature 32.0 - 312 °F |
Average value: 76.5 µm/m-°C Grade Count:4 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 45.0 - 90.0 µm/m-°C | 25.0 - 50.0 µin/in-°F | Average value: 63.7 µm/m-°C Grade Count:46 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
CTE, linear | 12.0 - 90.0 µm/m-°C | 6.67 - 50.0 µin/in-°F | Average value: 44.3 µm/m-°C Grade Count:14 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 17.1 - 90.0 µm/m-°C | 9.50 - 50.0 µin/in-°F | Average value: 48.4 µm/m-°C Grade Count:38 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
CTE, linear | 70.0 - 90.0 µm/m-°C | 38.9 - 50.0 µin/in-°F | Average value: 80.0 µm/m-°C Grade Count:4 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 32.0 - 90.0 µm/m-°C | 17.8 - 50.0 µin/in-°F | Average value: 67.0 µm/m-°C Grade Count:6 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
CTE, linear | 80.0 - 90.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
44.4 - 50.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX6601 PPE+PA66 (Asia Pacific) PPE+PA Unfilled GTX |
|||
CTE, linear | 80.0 - 90.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
44.4 - 50.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX GTX6601 PPE+PA66 (Asia Pacific) |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 20.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Zeus EFEP Tubing |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 20.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON EP-610AS ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON RP-4040 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON EP-541 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
CTE, linear | 40.0 - 90.0 µm/m-°C | 22.2 - 50.0 µin/in-°F | Average value: 72.0 µm/m-°C Grade Count:5 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 80.0 - 90.0 µm/m-°C | 44.4 - 50.0 µin/in-°F | |
Master Bond EP21TDC-2LO Two component, highly flexibilized epoxy resin compound Product Description: Master Bond Polymer System EP21TDC-2LO is a two component, highly flexible epoxy resin compound for high performance bonding, sealing, coating, and encapsulation. It is formulat.. |
|||
CTE, linear | 54.0 - 90.0 µm/m-°C | 30.0 - 50.0 µin/in-°F | Average value: 72.0 µm/m-°C Grade Count:5 |
Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 80.0 - 90.0 µm/m-°C | 44.4 - 50.0 µin/in-°F | ASTM D696 |
Guarniflon PTFE G458 Polytetrafluoroethylene 60% Bronze, 2% Carbon PTFE G Standard Compound with bronzeProperties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard .. |