Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 52.7 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 52.7 µm/m-°C
29.3 µin/in-°F
Hexcel® HexPly® F155 Epoxy Resin
HexPly® F155 is an advanced modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness and adhesive properties. HexPly..
Copyright © lookpolymers.com All Rights Reserved