Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.5 - 55.8 µm/m-°C | 7.50 - 31.0 µin/in-°F | Average value: 26.9 µm/m-°C Grade Count:10 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
CTE, linear | 19.8 - 55.8 µm/m-°C | 11.0 - 31.0 µin/in-°F | Average value: 34.2 µm/m-°C Grade Count:29 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear | 4.00 - 55.8 µm/m-°C | 2.22 - 31.0 µin/in-°F | Average value: 26.3 µm/m-°C Grade Count:21 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
CTE, linear | 26.0 - 55.8 µm/m-°C | 14.4 - 31.0 µin/in-°F | Average value: 35.8 µm/m-°C Grade Count:4 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |