Thermal Properties Metric English Comments
CTE, linear 61.0 µm/m-°C

@Temperature -30.0 - 100 °C
33.9 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
LyondellBasell Hifaxâ„¢ Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB252 medium high melt flow, 1,200 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has very well balanced processability, rigidi..
CTE, linear 61.0 µm/m-°C

@Temperature 20.0 °C
33.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
CTE, linear 61.0 µm/m-°C

@Temperature 20.0 °C
33.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
CTE, linear 61.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
33.9 µin/in-°F

@Temperature -22.0 - 176 °F
Borealis Method
Borealis Daplen™ EE108U Polypropylene TPO Compound
Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives..
CTE, linear 61.0 µm/m-°C

@Temperature 40.0 - 130 °C
33.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 7500 Phenolic, Granular, Compression Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
CTE, linear 61.0 µm/m-°C

@Temperature 20.0 °C
33.9 µin/in-°F

@Temperature 68.0 °F
Tra-Con Tra-Cast 3011 Semi-Flexible Clear Epoxy Casting Compound
TRA-CAST 3011 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life..
CTE, linear 61.0 µm/m-°C

@Temperature 20.0 °C
33.9 µin/in-°F

@Temperature 68.0 °F
Tra-Con Tra-Cast F311 Optically Transparent Semi-Flexible Casting System
TRA-CAST F311 is a clear, low viscosity epoxy formulation developed for molding, embedding, casting and potting applications where clarity, toughness, long pot-life and superior impact properties ar..
CTE, linear 61.0 µm/m-°C

@Temperature 20.0 °C
33.9 µin/in-°F

@Temperature 68.0 °F
Tra-Con Tra-Cast FS255 Flexible Clear Epoxy Casting Compound
TRA-CAST FS-255 is a clear, low viscosity, epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties -- good clarity, long pot..
CTE, linear 61.0 µm/m-°C

@Temperature 20.0 °C
33.9 µin/in-°F

@Temperature 68.0 °F
Trelleborg Emerson & Cuming Stycast® 2072 Two-Component Easy Mix Ratio Encapsulant
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, ..
CTE, linear 61.0 µm/m-°C

@Temperature 20.0 °C
33.9 µin/in-°F

@Temperature 68.0 °F
Trelleborg Emerson & Cuming Stycast® 2651-40/23LV Two-Component General Purpose Encapsulant
Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as ..
CTE, linear 61.0 µm/m-°C
33.9 µin/in-°F
ASTM D696
Unitika U-100 Engineering Plastic
CAS No: 26590-50-1Information provided by Unitika Ltd.
CTE, linear 61.0 µm/m-°C

@Temperature 20.0 °C
33.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Devcon Combo Wear FC Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
CTE, linear 61.0 µm/m-°C

@Temperature 20.0 °C
33.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Devcon Wear Guard (Fine Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
CTE, linear 61.0 µm/m-°C
33.9 µin/in-°F
Below Tg
Epoxy Technology EPO-TEK® 301-2 Optically Transparent Epoxy
Product Description: EPO-TEK® 301-2 is a two component optical, medical, and semiconductor grade epoxy resin, with low viscosity, long pot-life, and good handling characteristics.Advantages & Appli..
CTE, linear 61.0 µm/m-°C
33.9 µin/in-°F
Below Tg
Epoxy Technology EPO-TEK® 730 Unfilled Black General and Structural Grade Epoxy
Material Description: A two component, room temperature curing, general and structural grade epoxy. It can be used for adhesive, sealing, and encapsulating applications in medical, xray device, fil..
CTE, linear 61.0 µm/m-°C
33.9 µin/in-°F
90 Minute UV Cure; T<Tg; ASTM E831-93
3D Systems Accura® SI 40 Plastic for the SLA® 250 System
Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing ..
CTE, linear 61.0 - 104 µm/m-°C
33.9 - 57.8 µin/in-°F
Average value: 74.0 µm/m-°C Grade Count:8
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
CTE, linear 61.0 - 61.0 µm/m-°C

@Temperature 60.0 - 138 °C
33.9 - 33.9 µin/in-°F

@Temperature 140 - 280 °F
Average value: 61.0 µm/m-°C Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Copyright © lookpolymers.com All Rights Reserved