Thermal Properties Metric English Comments
CTE, linear 11.0 - 13.0 µm/m-°C

@Temperature -40.0 - 125 °C
6.11 - 7.22 µin/in-°F

@Temperature -40.0 - 257 °F
X/Y; IPC-TM-650.2.4.41
Park Electrochemical Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg
The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a..
CTE, linear 11.0 - 13.0 µm/m-°C

@Temperature 1000 °C
6.11 - 7.22 µin/in-°F

@Temperature 1830 °F
Chosun Refractories HRD-SNE Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 11.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
6.11 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-2 Alnico Magnetic Material
CTE, linear 11.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
6.11 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-3 Alnico Magnetic Material
CTE, linear 10.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-5S Alnico Magnetic Material
CTE, linear 10.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-8S Alnico Magnetic Material
CTE, linear 11.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
6.11 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-5 Alnico Magnetic Material
CTE, linear 11.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
6.11 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-5-7 Alnico Magnetic Material
CTE, linear 11.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
6.11 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-5DG Alnico Magnetic Material
CTE, linear 11.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
6.11 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-6 Alnico Magnetic Material
CTE, linear 10.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-6S Alnico Magnetic Material
CTE, linear 11.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
6.11 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-8 Alnico Magnetic Material
CTE, linear 10.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance A-2S Alnico Magnetic Material
CTE, linear 13.0 - 13.0 µm/m-°C

@Temperature 180 - 180 °C
7.22 - 7.22 µin/in-°F

@Temperature 356 - 356 °F
Average value: 27.9 µm/m-°C Grade Count:1
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Copyright © lookpolymers.com All Rights Reserved