Polymer Property : CTE, linear = 70.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 90.0 - 126 µm/m-°C
50.0 - 70.0 µin/in-°F
ASTM D696
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
CTE, linear 90.0 - 126 µm/m-°C
50.0 - 70.0 µin/in-°F
ASTM D696
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
CTE, linear 90.0 - 126 µm/m-°C

@Temperature 20.0 °C
50.0 - 70.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Rochling Engineered Plastics Polystone® PVDF Extruded Sheet
Information provided by Röchling Engineered Plastics.