Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 1330 µm/m-°C @Temperature 20.0 °C |
737 µin/in-°F @Temperature 68.0 °F |
|
Dow ISONATE™ 181 MDI Prepolymer ISONATE™ 181 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with sufficient glycol to allow easy handling down to 80°F. This medium-viscos.. |