Polymer Property : CTE, linear = 77.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
Below glass transition temp; ASTM D696
Performance Polymers IPS II PPL-A1050 PEKK (Polyetherketoneketone) Branched Standard Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
CTE, linear 77.0 µm/m-°C

@Temperature 20.0 °C
42.8 µin/in-°F

@Temperature 68.0 °F
Cured
Resin Technology Group UV-403 High Clarity, Structural Polycarbonate and PVC Bonder
UV 403 is a very fast UV curing adhesive developed for bonding a variety of plastics. Bond strengths on polycarbonate and rigid PVC usually exceed the strength of those substrates. Bond lines are cl..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
ASTM D696
Unitika AX-1500 Dry
AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
ISO 11359-2
Unitika CX-2500 PA6, Conditioned
Transparent nylonInformation provided by Unitika Ltd.
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
Below Tg
Tra-Con Tra-Bond 7560D Hydrolytically Stable Adhesive
TRA-BOND 7560D is an electrically insulating epoxy adhesive. This material has a 10 day work life and a medium viscosity for easy usage. There are also multiple cure options that make this product i..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
ISO 11359-2
Unitika CX-2500 PA6, Dry
Transparent nylonInformation provided by Unitika Ltd.
CTE, linear 77.0 µm/m-°C

@Temperature 20.0 °C
42.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Covestro Bayblend® 2953 Polycarbonate + ABS Blend, Automotive Plating
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® E2001-HV Electrically Conductive, Silver-Filled Epoxy
Product Description: EPO-TEK® E2001-HV Is a snap cure, two component, silver-filled die attach adhesive for semiconductor plastic IC packaging.Advantages & Application Notes:Snap cure adhesive or f..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® E3001-HV Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & ..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
Epoxyset Epoxiohm EO-30M-1 Electrically Conductive Epoxy Adhesive
EO-30M-1 is a two part, semi-rigid, silver filled, epoxy adhesive. EO-30M-1 exhibits superior adhesion to a wide variety of substrates including most metals, ceramics, glass and plastics.Information..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
3M VHB™ F9460PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
3M VHB™ F9473PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
CTE, linear 77.0 µm/m-°C

@Temperature 20.0 °C
42.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000
PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast me..
CTE, linear 77.0 µm/m-°C

@Temperature 0.000 - 50.0 °C
42.8 µin/in-°F

@Temperature 32.0 - 122 °F
DIN 5372
Lucite International SW Sanitary Ware Acrylic Sheet
Lucite® SW complies with ISO 7823-1 and EN 263. It is approved by the French ARNOR "NF" quality mark.Information provided by Lucite International
CTE, linear 77.0 µm/m-°C

@Temperature 20.0 °C
42.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..