Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 78.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 78.0 µm/m-°C

@Temperature 20.0 °C
43.3 µin/in-°F

@Temperature 68.0 °F
NOVA Chemicals Laboratory Procedure
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
CTE, linear 78.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
43.3 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2; Parallel to Flow
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade
Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food..
CTE, linear 78.0 µm/m-°C

@Temperature 20.0 °C
43.3 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Lucite International Perspexâ„¢ XT Acrylic Extruded Sheet 0X00
PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information..
CTE, linear 78.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
CTE, linear 78.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
CTE, linear 78.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
CTE, linear 78.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
CTE, linear 78.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
CTE, linear 78.0 µm/m-°C
43.3 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® H20-LC Electrically Conductive, Silver Epoxy
Product Description: EPO TEK® H20E-LC is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also used exte..
CTE, linear 78.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
CTE, linear 78.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
43.3 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228
Solvay Engineered Polymers DEXFLEX® 900 TPO  (discontinued **)
Description: DEXFLEX® 900 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paint..
Copyright © lookpolymers.com All Rights Reserved