Polymer Property : CTE, linear = 80.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 72.0 - 144 µm/m-°C
40.0 - 80.0 µin/in-°F
Average value: 94.5 µm/m-°C Grade Count:17
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
CTE, linear 6.00 - 144 µm/m-°C

@Temperature 50.0 - 300 °C
3.33 - 80.0 µin/in-°F

@Temperature 122 - 572 °F
Average value: 48.7 µm/m-°C Grade Count:29
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
CTE, linear 54.0 - 144 µm/m-°C

@Temperature 25.6 - 204 °C
30.0 - 80.0 µin/in-°F

@Temperature 78.0 - 400 °F
ASTM D696
Technetics Group Texolon™ 9406 PTFE  (Unverified Data**)
General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel..
CTE, linear 54.0 - 144 µm/m-°C

@Temperature 25.6 - 204 °C
30.0 - 80.0 µin/in-°F

@Temperature 78.0 - 400 °F
ASTM D696
Garlock 9405 PTFE Rubber Sheet, 25% Glass Filled
Premium Grade 25% Glass-filled Skived PTFE SheetInformation provided by Garlock Rubber Technologies
CTE, linear 90.0 - 144 µm/m-°C

@Temperature 20.0 °C
50.0 - 80.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Zeus PVDF Tubing
PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char..
CTE, linear 119 - 144 µm/m-°C
66.0 - 80.0 µin/in-°F
ASTM D696
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
CTE, linear 119 - 144 µm/m-°C
66.0 - 80.0 µin/in-°F
ASTM D696
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
CTE, linear 119 - 144 µm/m-°C
66.0 - 80.0 µin/in-°F
ASTM D696
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
CTE, linear 119 - 144 µm/m-°C
66.0 - 80.0 µin/in-°F
ASTM D696
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
CTE, linear 119 - 144 µm/m-°C
66.0 - 80.0 µin/in-°F
ASTM D696
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..