Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | DIN.52612 (dry sample) |
Omnia Plastica Akulon® PA 66.6 - Akulon GX - at 50% RH Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tool.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | DIN.52612 |
Omnia Plastica PSU Polysulphone It is a non-reinforced amorphous polymer whose main features are its high thermal, electrical and mechanical properties which are typical of a crystalline polymer. Compared to its "brother" PES it h.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8301:1991 |
Global EPP PA 6C Cast Polyamide 6 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PSU Polysulfone Electrical insulating productsRigidHigh chemical, fire and temperature resistanceInformation provided by Isoflon. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV511 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DEBT (deputy tin deflagrate) as the stan.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 1110F PEI (Europe-Africa-Middle East) Enhanced flow PolyetherimiEnhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no long.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Solvay Chemicals Polyglycerol-3 A polyglycerol characterized by a very narrow oligomer distribution centered on triglycerol.EINECS Number: 915-741-3/CAS Number: 25618-55-7Information provided by Solvay |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI) Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI) Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl PX1115 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1115 is an unfilled, flame retardant material with a Vicat B/120 of 140°C according ISO 306. NORYL PX1115 is V1 at 1.2 mm according UL94 and halogen free according VDE/DIN 472 part 815.Th.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Styron Pulse® EXT 100 ABS + Polycarbonate PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering .. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East) NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6 Zytel 73G45 BK263 is a 45% glass fiber reinforced black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Elisto THERMOSTAR® LC 350 Si Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 103 PTFE, 10% Carbon Filled Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C-177 |
Glastic GLASGUARD Scuff and Bulkhead Liners GlasGuard Scuff and Bulkhead Liners serve as a method of protecting trailer walls from damage caused by forklift trucks and careless loading and unloading of freight. Manufactured of 1/4" thick fib.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Europe-Africa-Middle East) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | Melt; ASTM C177 |
Styron PULSE™ EXT 100 PC/ABS Engineering Resin Overview: PULSE EXT 100 engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT 100 engin.. |
|||
Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 305 PTFE, 15% Graphite Information provided by Adamas, HPM |