Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.282 - 0.513 W/m-K | 1.96 - 3.56 BTU-in/hr-ft²-°F | Average value: 0.407 W/m-K Grade Count:4 |
Overview of materials for Phenolic, Ablative Coating This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Ablative Coating". Each property range of values reported is minimum and maximum values of app.. |
|||
Thermal Conductivity | 0.282 W/m-K | 1.96 BTU-in/hr-ft²-°F | |
Haveg 41NA Phenolic; Silicate Filled A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers. |