Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 1.45 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Honeywell ACLAR® 11A (3.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Honeywell ACLAR® 11A (2.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV102 One Component Acetoxy Adhesive Sealant, White
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV108 One Component Acetoxy Adhesive Sealant, Translucent
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV109 One Component Acetoxy Adhesive Sealant, Aluminum
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV112 One Component Acetoxy Adhesive Sealant, White
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV116 One Component Acetoxy Adhesive Sealant, Red
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV118 One Component Acetoxy Adhesive Sealant, Translucent
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray
RTV 157 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red
RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White
RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV162 Electronic Grade Silicone Adhesive Sealant, White
RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV167 Electronic Grade Silicone Adhesive Sealant, Gray
RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Momentive Performance Materials RTV1673LV One Component, Low Volatile Silicone Adhesive Sealant, Black
RTV1673LV one-component, ready-to-use adhesive sealants cures to a tough durable, resilient silicone rubber when exposed to atmospheric moisture at room temperature. Methyl alcohol and a small amoun..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
ASTM C177-76
Lucite International XL Sanitary Ware Acrylic Sheet
Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Cento-Fitch
Spartech Polycast SAR (Super Abrasion Resistant) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
ASTM D177
Diapolyacrylate Acrypet® MF-001 PMMA
Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers.
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
ASTM D177
Diapolyacrylate Acrypet® VH-001 Heat Stabilized PMMA
Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers.
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
ASTM D177
Diapolyacrylate Acrypet® IR H70 Impact Modified PMMA
Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers.
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa..
Thermal Conductivity 0.209 W/m-K
1.45 BTU-in/hr-ft²-°F
Arlon R33889R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Layer-on-Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information ..
Copyright © lookpolymers.com All Rights Reserved