Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FE-5620Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FC-2122 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good flow, release and hot tear for c.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FC-2123 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent hot tear and compression se.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FC-2178 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FC-2261Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Algoflon® S 131 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.2 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/BK Polyamide 66, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/HS-B Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Heat stabilised.High dimension.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1-0935 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Algoflon® F 7 Polytetrafluoroethylene (PTFE) Algoflon® F 7 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for normal compression molding and in particular molding of large billets for low .. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem ATX100R PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB Listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM PW2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 1000P PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. Resin is RoHS compliant. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PA (Europe-Africa-Middle East) NORYL GTX810 is a 10% glass reinforced grade with excellent chemical resistance in combination with high stiffness and high heat resistance. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Borealis RA130E Polypropylene Random Copolymer RA130E is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is natural colored. Applications RA130E is recommended for the production of PP-R pipes and .. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |
|||
Thermal Conductivity | 0.240 W/m-K @Temperature 1400 °C |
1.67 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia Buster A-30 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | Moulding Direction; ASTM C177 |
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static) Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Thermal Conductivity | 0.241 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
Ensinger Tecast Vekton™ 6PA Blue Unfilled Cast Nylon 6 (PA6) Tecast 6PA Blue is a blue cast nylon with properties similar to natural nylon 6.General Tecast Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of go.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Algoflon® A.27 PTFE (Polytetrafluoroethylene)