Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.65 W/m-K | 11.5 BTU-in/hr-ft²-°F | |
Loctite® 3873 1 component acrylic High Conductivity Flexible Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Thermal Conductivity | 1.65 W/m-K | 11.5 BTU-in/hr-ft²-°F | in plane; ASTM E1461 |
DSM Arnite® AV2 370 XL-T PET-GF35 35% Glass Reinforced, Low Outgassing, Thermal conductive material |