Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | >= 2.00 W/m-K | >= 13.9 BTU-in/hr-ft²-°F | |
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative NanoTach® is a thick paste of nano-sized silver powder in an organic binder that can be used as an alternative to solder or epoxy in semiconductor devices in the state-of-the-art individual package.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | ASTM E-1461 |
Ovation Polymers Nemcon™ H PC DP111/X1 Polycarbonate Polycarbonate-Thermally and electrically conducting grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
GBC 496 Alumino Silicate Ceramic Propriety composition with CTE equivalent to Pyrex® glass. Can seal directly to 7070 glass, Pyrex®, or other grades of silicon. Has excellent thermal shock resistance, low firing temperature.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
McDanel Advanced Ceramics Z105 Yttria stabilized Zirconia Information provided by McDanel Advanced Ceramic Technologies |
|||
Thermal Conductivity | 2.00 W/m-K @Temperature 800 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
McDanel Advanced Ceramics Z105 Yttria stabilized Zirconia Information provided by McDanel Advanced Ceramic Technologies |
|||
Thermal Conductivity | 2.00 - 10.0 W/m-K | 13.9 - 69.4 BTU-in/hr-ft²-°F | |
MetaFoam Copper Foam General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional†metal foams. MetaFoam can .. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Misumi Steatite MgO-SiO2Information provided by MISUMI Corporation. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | in "c" direction |
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 .. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain Vitreosil® 055 Optical Fused Quartz Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | DIN EN 821-2 / ASTM-C408 |
CeramTec Sikor® E Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® EJ2189-LV Electrically Conductive Epoxy Low Viscosity, two component room temp curing conductive epoxyInformation Provided by Epoxy Technology |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Epoxyset Epoxiohm EO-30FST Electrically Conductive Epoxy Adhesive EO-30-FST is two part, fast cure, silver filled, and high electrical conductivity epoxy adhesive. Both components are silver filled permitting a simple 1:1 mix ratio by weight. It has smooth creamy .. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Epoxyset Epoxiohm EO-30M-1 Electrically Conductive Epoxy Adhesive EO-30M-1 is a two part, semi-rigid, silver filled, epoxy adhesive. EO-30M-1 exhibits superior adhesion to a wide variety of substrates including most metals, ceramics, glass and plastics.Information.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Advanced Ceramics ACL 2089 Cordierite Cordierite glass-ceramic has good thermal shock properties and is suitable for heat resistant components which undergo rapid thermal cycling.Information provided by Advanced Ceramics Limited (ACL) |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Alliance BCN-13 Bonded (Composite) Magnetic Material |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Alliance BCN-12 Bonded (Composite) Magnetic Material |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Alliance BCN-14 Bonded (Composite) Magnetic Material |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Alliance BCN-15 Bonded (Composite) Magnetic Material |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Alliance BCN-17 Bonded (Composite) Magnetic Material |
|||
Thermal Conductivity | 2.00 W/m-K @Temperature 20.0 - 100 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized Available in impervious or porous grades in a range of shapes and sizes.Information provided by Anderman Ceramics. |