Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4303 Cr-Ni Austenitic Stainless Steel Good corrosion resistance with excellent drawing properties.Applications: Suitable for cold formed components where good workability is required. Fasteners, studs.Available in hot rolled plate (Qua.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4305 Austenitic Stainless Steel Good general corrosion resistance.Applications: Where machinability is required - threaded bar, studs, domestic appliances.Available in bar and rod forms. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 85.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy 140 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 85.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 117 Bi-Pb-In-Sn-Cd Fusible Alloy General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 - 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 - 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 - 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10 LN Nitrogen Containing 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18.10LN is a 18Cr-10Ni austenitic stainless steel with specific Nitrogen additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior .. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 - 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 - 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 52/11 GR/70 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS327 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | |
Cytec Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | |
Cytec Thornel® T-650/42 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | |
Cytec Thornel® T-650/42 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | Fiber Value |
Cytec Thornel® VCB-20 Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Used as a reinforcement in structural, ablative, and abrasion-resistant composites.2000 filaments/strand, 99+% carbon assayThornel®.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | |
Resistalloy International Resistalloy 8020 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum.. |