Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, cold worked sheet, 15% cold reduction, aged at 370°C (700°F) for 1 hour Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, cold worked sheet, 20 % cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, hot rolled and 1230°C solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 20% cold reduction, 1175°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 25% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 25% cold reduction, 1065°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 25% cold reduction, 1120°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 25% cold reduction, 1175°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature sheet after 100 hours of 760°C exposure Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature sheet after 100 hours of 870°C exposure Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature sheet after 1000 hours of 650°C exposure Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature sheet after 1000 hours of 870°C exposure Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature sheet after 2500 hours of 650°C exposure Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature sheet after 500 hours of 650°C exposure Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature sheet after 500 hours of 870°C exposure Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Thermal Conductivity | 26.6 W/m-K @Temperature 100 °C |
185 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM-C408 |
CoorsTek ADS-996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 0% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 10% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 10% cold reduction, 1065°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 10% cold reduction, 1175°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 15% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 15% cold reduction, 1120°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 15% cold reduction, 1175°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 20% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 20% cold reduction, 1065°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 20% cold reduction, 1120°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 10% cold reduction, 1120°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Thermal Conductivity | 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 25 alloy, room temperature after 15% cold reduction, 1065°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |