Polymer Property : Thermal Conductivity = 19.0 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity >= 2.74 W/m-K
>= 19.0 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® P1011 Electrically Conductive Modified Polyimide
Product Description: EPO-TEK® P-1011 is a single component, modified polyimide, silver-filled adhesive designed for chip bonding in microelectronic and optoelectronic applications.Advantages & Appl..