Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | >= 2.00 W/m-K | >= 13.9 BTU-in/hr-ft²-°F | |
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative NanoTach® is a thick paste of nano-sized silver powder in an organic binder that can be used as an alternative to solder or epoxy in semiconductor devices in the state-of-the-art individual package.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | ASTM E-1461 |
Ovation Polymers Nemcon™ H PC DP111/X1 Polycarbonate Polycarbonate-Thermally and electrically conducting grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
Thermal Conductivity | 2.00 - 3.00 W/m-K | 13.9 - 20.8 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Therma-Tech™ NJ-6000C TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
McDanel Advanced Ceramics Z105 Yttria stabilized Zirconia Information provided by McDanel Advanced Ceramic Technologies |
|||
Thermal Conductivity | 2.00 - 10.0 W/m-K | 13.9 - 69.4 BTU-in/hr-ft²-°F | |
MetaFoam Copper Foam General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional†metal foams. MetaFoam can .. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | in "c" direction |
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi.. |
|||
Thermal Conductivity | 2.00 - 10.0 W/m-K | 13.9 - 69.4 BTU-in/hr-ft²-°F | |
MetaFoam Copper-Silver Foam General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional†metal foams. MetaFoam can .. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 47/1 CP/80 PP Copolymer High thermal conductivity product based on Polypropylene copolymer (PPc). Special filler. Extrusion and molding injection grade.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain HS Grade Optical Fused Quartz HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, .. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain Vitreosil® 055 Optical Fused Quartz Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures... |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Sapco Partially Stabilized TZP Zirconia (YSZ) Information provided by Sapco. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® EJ2189-LV Electrically Conductive Epoxy Low Viscosity, two component room temp curing conductive epoxyInformation Provided by Epoxy Technology |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Epoxyset Epoxiohm EO-30M-1 Electrically Conductive Epoxy Adhesive EO-30M-1 is a two part, semi-rigid, silver filled, epoxy adhesive. EO-30M-1 exhibits superior adhesion to a wide variety of substrates including most metals, ceramics, glass and plastics.Information.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Epoxyset Epoxiohm EO-38M-3 Electrically Conductive Epoxy Adhesive EO-38M-3 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management appl.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Alliance BCN-11 Bonded (Composite) Magnetic Material |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Alliance BCN-13 Bonded (Composite) Magnetic Material |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive AA-SUPERTHERM 195 is a two component, thermally conductive epoxy system recommended for staking transistors, diodes, resistors, integrated circuits and other heat sensitive components to printed cir.. |
|||
Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
Alliance BCN-17 Bonded (Composite) Magnetic Material |
|||
Thermal Conductivity | 2.00 W/m-K @Temperature 20.0 - 100 °C |
13.9 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized Available in impervious or porous grades in a range of shapes and sizes.Information provided by Anderman Ceramics. |