Polymer Property : Thermal Conductivity = 2.18 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.314 W/m-K
2.18 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 9 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 0.314 W/m-K
2.18 BTU-in/hr-ft²-°F
ASTM F433
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F..