Thermal Properties Metric English Comments
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel
Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms.
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4439 Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms.
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4501 Duplex Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Thermal Conductivity 20.0 - 24.9 W/m-K
139 - 173 BTU-in/hr-ft²-°F
ASTM C177
PolyOne Therma-Tech™ NJC-7500 TC Nylon 12  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Thermal Conductivity 20.0 W/m-K
139 BTU-in/hr-ft²-°F
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel
Description: S692/S693 MICROCLEAN are high-sulfur and low sulfur versions of high-carbon PM M4 high speed steel that is produced using state-of-the-art “Generation 3” powder processing technology...
Thermal Conductivity 20.0 W/m-K
139 BTU-in/hr-ft²-°F
Bohler-Uddeholm BÖHLER S500(m42) High Speed Steel
Description: Cobalt Molybdenum high speed steel processing high hardness, excellent cutting properties, high red hardness and good toughness. BOHLER S500 is also available in the special grade ISORA..
Thermal Conductivity 20.0 W/m-K
139 BTU-in/hr-ft²-°F
perpendicular
Carlisle 201HL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Thermal Conductivity 20.0 - 120 W/m-K
139 - 833 BTU-in/hr-ft²-°F
in "ab" direction
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating
High temperature protective coating for graphite.PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite fr..
Thermal Conductivity 20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..