Polymer Property : Thermal Conductivity = 3.10 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.447 W/m-K

@Temperature 23.9 °C
3.10 BTU-in/hr-ft²-°F

@Temperature 75.0 °F
ASTM F-433
PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole
Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. ..