Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 50.0 - 200 W/m-K | 347 - 1390 BTU-in/hr-ft²-°F | |
NanoAmor 50% Regular Single Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption an.. |
|||
Thermal Conductivity | 50.0 - 200 W/m-K | 347 - 1390 BTU-in/hr-ft²-°F | |
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Thermal Conductivity | 50.0 W/m-K @Temperature 85.0 °C |
347 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation. |
|||
Thermal Conductivity | 50.0 W/m-K @Temperature 85.0 °C |
347 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® Sn62 Sn-Pb-Ag Solder Alloy Good general purpose solder. Can be used on silver bearing surfaces to reduce scavenging.Information provided by the manufacturer, Indium Corporation. |
|||
Thermal Conductivity | 50.0 W/m-K @Temperature 85.0 °C |
347 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy 104 Tin-Lead Solder Alloy Widely used electronic solder. Good for silver metallization. Has improved strength and fatigue propertiesInformation Provided by Indium Corporation |
|||
Thermal Conductivity | 50.0 W/m-K | 347 BTU-in/hr-ft²-°F | ASTM E1461 |
M Cubed Technologies RBBC-751 Reaction Bonded Boron Carbide Reaction-bonded boron carbide for extreme wear environments. Can be cast into very large components (greater than 4 ft. square)Information provided by M Cubed Technologies, Inc. |
|||
Thermal Conductivity | 50.0 - 100 W/m-K | 347 - 694 BTU-in/hr-ft²-°F | Perpendicular to Plane |
Goodfellow Carbon-Carbon Composite Carbon Fiber - Carbon MatrixInformation provided by Goodfellow. |
|||
Thermal Conductivity | 50.0 - 75.0 W/m-K | 347 - 521 BTU-in/hr-ft²-°F | |
Goodfellow Phosphor Bronze Good Machinability. Uses include springs, clips, gauzes and architectural applicationsInformation provided by Goodfellow. |
|||
Thermal Conductivity | 50.0 W/m-K | 347 BTU-in/hr-ft²-°F | ASTM-C408 |
CoorsTek Boron Carbide Reaction-Bonded Boron Carbide Lowest density for ultra-lightweight designs |
|||
Thermal Conductivity | 50.0 W/m-K | 347 BTU-in/hr-ft²-°F | in plane |
Carlisle 201HL Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |