Polymer Property : Thermal Conductivity = 597 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 86.0 W/m-K

@Temperature 85.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 4 Pure Indium Solder
Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogeni..
Thermal Conductivity 86.0 W/m-K
597 BTU-in/hr-ft²-°F
Special Metals Nickel 270
A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele..
Thermal Conductivity 86.0 W/m-K
597 BTU-in/hr-ft²-°F
Tokuyama Shapal™ SH-50 Sintered Aluminum Nitride
Uniform, large sized pressed sintered aluminum nitride.
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899A 1/2 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899A 1/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899A 3/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899A Full Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899A Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899D 50% Cold-Rolled
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899D Annealed
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899E 50% Cold-Rolled
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899E Annealed
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899L 1/2 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899L 1/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899L 3/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899L Annealed
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899L Full Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899L Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899L Skin Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899M 1/2 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899M 1/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899M Annealed
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899M Full Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899M Skin Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899A Annealed
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899A Skin Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899G 50% Cold-Rolled
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899G Annealed
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899M 3/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Ametek High Purity Nickel Strip 899M Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..