Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | in-plane, ø25*0.4mm disc; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX09322 PA 6 (Asia Pacific) White colored thermally conductive mineral filled PA6 FR compound |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | JIS-R-2618; ASTM D2326 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | 120°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | 150°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | 60°C for 1,000 hrs with 90% RH; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | 70°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | JIS-R-2618; ASTM D2326 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | 120°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | 150°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | 60°C for 1,000 hrs with 90% RH; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | 70°C for 1,000 hrs; JIS-R-2618 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | |
McDanel Advanced Ceramics MV-30 Mullite Information provided by McDanel Advanced Ceramic Technologies |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | Through Thickness; ASTM-D5470 Modified (at 110kPa/16 psi/1.1 bar) |
GrafTech eGRAF® HITHERM™ HT-705 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | Through Thickness; ASTM-D5470 Modified (at 110kPa/16 psi/1.1 bar) |
GrafTech eGRAF® HITHERM™ HT-710 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | Through Thickness; ASTM-D5470 Modified (at 110kPa/16 psi/1.1 bar) |
GrafTech eGRAF® HITHERM™ HT-720 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | across thickness |
Ultracor® UCF-51-3/8-2.0 Honeycomb Core Material Construction: ±45° XN50. Fiber: Carbon XN50. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures. It is expected that it will be use.. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | |
Cytec Thornel® VCK Carbon Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | |
Cytec Thornel® VCK Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | |
Cytec Thornel® VCL Carbon Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Thermal Conductivity | 6.00 W/m-K | 41.6 BTU-in/hr-ft²-°F | |
Cytec Thornel® VCL Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |