Thermal Properties Metric English Comments
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 2 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 45 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1018, Grade 30 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1018, Grade 36 Type 1 and 2 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ASTM A 424 Type II, VIT-PLUS® DS Enameling Carbon Steel
VIT-PLUS is a controlled chemistry, non-decarburized steel designed to replace certain types of ingot products. It has good strength after fire properties. It is not recommended for direct-on cove..
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ASTM A 607 Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec..
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ASTM A 607 Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec..
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ASTM A 607 Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec..
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ASTM A 607 Class 1 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec..
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ASTM A 607 Class 2 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. ..
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ASTM A 607 Class 2 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. ..
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ASTM A 715 Class 2 Formable, Grade 50F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 715 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. ..
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ASTM A 715 Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 715 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. ..
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel CL 1/ SAE J1392 045 XLK, Grade 50 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel CL 2/ SAE J1392 045 XLK, Grade 50 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel SAE J1392 040XLK or 040YLK, Grade 40 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel SAE J1392, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, HSLAS, FORMABLE 40K / SAE J1392 040 XLK or 040 YLK
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 1 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, High Strength Low Alloy Steel (HSLA), 040XLK
SAE Specified properties not covered by ASTMInformation provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 1 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 2 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 30 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 33 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K

@Temperature 20.0 °C
618 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 40 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel SAE J1392, Grade 50F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
AK Steel SAE J1392, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel