Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | a direction |
MarkeTech Rutile (TiO2) Fiber Optic Crystal More chemically and physically resistant than Yttrium Vanadate. Large birefringence. Used for fiber optic beam displacers and optical isolators. Grown by Vernull method. Transmission range 500 to.. |
|||
Thermal Conductivity | 9.00 W/m-K @Temperature 85.0 °C |
62.5 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 261 Bismuth-Silver Solder Alloy Information provided by the manufacturer, Indium Corporation of America. |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Special Metals UDIMET® alloy R41 Ni-Cr Alloy UDIMET® alloy R41 (UNS N07041) is a precipitation-hardenable nickel-chromium alloy containing significant amounts of cobalt and molybdenum, along with lesser amounts of aluminum and titanium. Al.. |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Cytec Thornel® P-650/35 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Cytec Thornel® P-650/42 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-28EH Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-28UH Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-30EH Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-30UH Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-35 Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-35M Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-38SH Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-40H Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-40SH Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-42 Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-42M Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-44H Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-45 Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-50 Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-30EZ Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-33 Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-33H Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-33SH Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-33UH Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-38H Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-38M Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-40 Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-42H Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-33M Neodymium Iron Boron Magnetic Material |
|||
Thermal Conductivity | 9.00 W/m-K | 62.5 BTU-in/hr-ft²-°F | |
Alliance N-48 Neodymium Iron Boron Magnetic Material |