Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 115 °C @Time 1.80e+7 sec |
239 °F @Time 5000 hour |
Continuous |
Nylacast H.S. Blue Cast Nylon 6, Heat Stabilized HS Blue is a heat Stabilised Cast Nylon 6. Its mechanical properties are maintained when operating at higher temperature and improves mechanical properties. This helps to reduce the stress distortio.. |
|||
Maximum Service Temperature, Air | 115 °C @Time 1.80e+7 sec |
239 °F @Time 5000 hour |
Continuous |
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Deflection Temp.; ASTM D648 |
NCMT NanoPAC™ S201 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Electrical Appliances AutomobileInformation provided by Nano Composi.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Deflection Temp.; ASTM D648 |
NCMT NanoPAC™ S202 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 W-KF30 Nylon 6 for injection molding, 30% short glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; 5,000 h |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; 5,000 h |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 GV40 Nylon 6 for injection molding, 40% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 H-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 W-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Electrical |
CE Phenolic Laminate Cotton based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many s.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Electrical |
LE Phenolic Laminate Linen based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many st.. |
|||
Maximum Service Temperature, Air | 115 - 254 °C | 239 - 489 °F | Average value: 179 °C Grade Count:5 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | 5000 hours; 50% Tensile Strength; IEC 216; DIN 53446 |
Zell-Metall Engineering Plastics Zellamid 1400 (PET) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | 5000 hours; 50% Tensile Strength; IEC 216; DIN 53446 |
Zell-Metall Engineering Plastics Zellamid 1400 (PET) at 50% RH Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | 5000 hours; 50% Tensile Strength; IEC 216; DIN 53446 |
Zell-Metall Engineering Plastics Zellamid 1400T (PET + solid lubricant) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Bond F125 Fast Gel Clear Epoxy Adhesive TRA-BOND F125 is a 10 minute gelling epoxy recommended for use in fiber optic connectors, optical and industrial bonding applications. This clear, two part system is easily mixed and used at room te.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Bond FS420 Flexible Plastic Adhesive TRA-BOND FS-420 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or almost any thermopl.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Bond 2106 Fast Cure, Medium Viscosity Epoxy Adhesive TRA-BOND 2106 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This clear, two-part, medium viscosity syste.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | short term; EMS |
EMS-Grivory Grivory® TR 90 NZZ nat PAMACM12-I Product description: Grilamid TR 90 NZZ natural is an amorphousthermoplastic polyamide, based on aliphatic and cycloaliphatic units. Grilamid TR 90 NZZ natural offers a variety of interesting proper.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Service |
3M FMV02 Void Polyester Label Products 3M™ Void Polyester Label Products are tamper-indicating stocks designed to provide a “void” message in the facestock when removal is attempted. These void polyester labels utilize 3M™ Adhesive P.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Service |
3M FMV01402 Triangle Void Polyester Label Products 3M™ Triangle Void Polyester Label Products FMV01202 and FMV01402 are a tamper-indicating stock designed to provide a triangle pattern in the facestock when removal is attempted. These label product.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Atom Adhesives AA-BOND F125 Epoxy Adhesive AA-BOND F125 is a 8 minutes gelling epoxy recommended for use in fiber optic connectors, optical and industrial bonding applications. AA-BOND F125 is clear, two part system is easily mixed and used .. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Atom Adhesives AA-SUPERTHERM 05 Epoxy Adhesive AA-SUPERTHERM 05 is a thixotropic (smooth paste) Pure Diamond ultra-high thermally conductive epoxy two-part adhesive that develops strong, durable, high-impact bonds at room temperature which impro.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Long Term |
CENTROPLAST CENTROLYTE ZX Polyethylene terephthalate with lubricant This material's solid lubricant additive has good sliding properties, and is well suited for high load, dry running situations. Possible uses include precision plain bearings, plug connectors, r.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous Use |
Polyram PlusTek RA320G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous Use |
Polyram PlusTek RA321G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Long Term |
CENTROPLAST CENTROLYTE Polyethylene terephthalate This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance. Applications include pump components, coil bodies, ball bearing cups and prote.. |