Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 125 °C | 257 °F | Recommended |
Nye Lubricants 174A (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Recommended |
Nye Lubricants 363F-WHITE (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Recommended |
Nye Lubricants 715 (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Recommended |
Nye Lubricants 760A (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Recommended |
Nye Lubricants 790DMS (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Precision Polymer Engineering C70R Chloroprene Rubber Red Iron Oxide filled, Chloroprene Rubber, 66-75 °IRHD. Flame retarding.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils. .. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
NextGen Adhesives P907-26 Optical Assembly Adhesive Description: NGAC P907-26 is a low viscosity and room temperature curing adhesive specifically formulated for optical applications where clarity is critical.Advantages and Applications: Uses include.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL A63 W-GV30 Nylon 6.6, std. viscosity for injection molding, 30% glass fiber reinforced Nylon 6.6, std. viscosity for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Parker Chomerics CHO-SEAL E6434 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Parker Chomerics Tecknit Teckfip™ FIP-E Formed in Place Conductive Elastomer Commercial grade FIP compound designed for moderate shielding performance. The Ag/glass particles are very smooth which leads to very low compression set value. The material is also available as a h.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Resin Technology Group 1105 Oxy-Bond™ Two-Component Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Precision Polymer Engineering C90B Chloroprene Rubber Chloroprene Rubber, 86-95 °IRHD. To meet British Standard BS5176 line call-out M2BC907.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleu.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 V0 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Humiseal 2A64 Urethane Conformal Coating Humiseal 2A64 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-46058C)F.. |
|||
Maximum Service Temperature, Air | 125 - 135 °C | 257 - 275 °F | Softening Range |
Huntsman Araldite GT 6097 US Bisphenol A Epoxy Solid Resin Weight per Epoxide (EEW, g/eq) 2000 to 2500. Max color is 3.Comments/Applications: Unmodified bis A "Type 7" epoxy. Higher melt viscosity "Type 7" for high quality industrial and thick film powder.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Industrial Laminates/Norplex NP310 Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500". |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Ball Pressure Temperature; IEC 60695-10-2 |
Mitsubishi Xantar® 18 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
LATI Latamid 66 H2 G/35-V0HF1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
LATI Latene® AG7H2 G/50 PP Homopolymer, 50% Glass Fiber Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
ELASTO UK Dryflex® 600750S SEBS Based Material, Filled Qualities, 75A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
ELASTO UK Dryflex® 662450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
ELASTO UK Mediprene™ 500750M TPE, Medical Applications, 75A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Service |
3M FM027 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Service |
3M FM030 Indoor UL Recognized Clear Polyester Label Products on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Service |
3M FM035 Indoor UL Recognized Clear Polyester Label Products on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Service |
3M FM072 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Matte Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester ov.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Atom Adhesives AA-BOND 2104 Epoxy Adhesive AA-BOND 2104 is a thixotropic epoxy system recommended for critical electronics, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Service |
3M FM023 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Ball Pressure Temperature; IEC 60695-10-2 |
Mitsubishi Xantar® MX 1004 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |