Thermal Properties Metric English Comments
Maximum Service Temperature, Air 760 °C
1400 °F
Not recommended for use in continuous casting applications.
Pyrotek Pyrocast AR Castable Refractory
Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro..
Maximum Service Temperature, Air 760 °C
1400 °F
Exception: Not recommended for use in continuous casting applications.
Pyrotek Pyrocast AR FINE Castable Refractory
Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall casting..
Maximum Service Temperature, Air 760 °C
1400 °F
intermittent
Pyrotek Pyrocast AR LITE Castable Refractory
A light weight highly insulating refractory product which offers excellent resistance to molten aluminum erosion and thermal shock.ApplicationsFor conveyance and casting of aluminum and its alloys A..
Maximum Service Temperature, Air 760 °C
1400 °F
Pyrotek T-20 Fiberglass Fabric
Close woven fiberglass. Does not cause severe skin irritation. Lightweight, light-brown, chemical resistant fabric.Information provided by Pyrotek.
Maximum Service Temperature, Air 760 °C
1400 °F
Continuous
Mid-Mountain Materials HYTEX® 1400 Fiberglass Industrial Textile
Description: Hytex is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying che..
Maximum Service Temperature, Air 760 °C
1400 °F
<100 hr, depends on temperature gradient
Schott ROBAX® Glass Ceramic
ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled s..
Maximum Service Temperature, Air 760 °C
1400 °F
Used as a non-conducting structural component up to this temp.
Von Roll Isola IMI MICA MAT® Inorganic Bonded Mica Plate
Data provided by Von Roll Isola USA.Rigid plate designed for use as a non-conducting structural component up to 760°C. 100% inorganic so it maintains good physical and electrical properties at ele..
Maximum Service Temperature, Air 760 °C
1400 °F
XADC-Armoloy Diamond-Chrome Composite Coating
XADC-Armoloy® combines the Armoloy® TDC chromium coating with spherical diamond particulates. The XADC-Armoloy® coating enhances the durability of components used in a wide range of applications..
Maximum Service Temperature, Air 760 °C
1400 °F
Recommended Operating Temperature
Unifrax Fiberfrax® Fiberwall® 304 SS Systems Hardware
The Fiberwall® systems family of anchoring hardware and accessory components provides an array of attachment options to cover a broad range of lining system designs and application requirements. I..
Maximum Service Temperature, Air 760 °C
1400 °F
Significant oxidation resistance to this temp.
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930
Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive ..
Maximum Service Temperature, Air 760 °C
1400 °F
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F.
Maximum Service Temperature, Air 760 °C
1400 °F
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F.
Maximum Service Temperature, Air 760 °C
1400 °F
BNZ Materials 375 Insulating Cement
375 Finishing Cement is a one coat finish which hardens to a smooth, crack-free surface in a few hours. This surface may then be painted with a water-base paint. Recommended for insulating small ste..
Maximum Service Temperature, Air 760 °C
1400 °F
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Maximum Service Temperature, Air 760 °C
1400 °F
Aremco Pyro-Putty™ 1000 High Temperature Ceramic-Metallic Putty, Aluminum Filled
Ceramic and Aluminum-Filled, Two-Part, Water Based Paste.For Applications to 1/2" Thick.Repairs Cast Aluminum Parts to 1400°F
Copyright © lookpolymers.com All Rights Reserved