Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1525 °C | 2777 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 80 A Dense Refractory Brick Description: A 78% alumina, bauxite based, quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from s.. |
|||
Maximum Service Temperature, Air | 1525 °C | 2777 °F | |
Gouda Vuurvast AK 80 A Dense Refractory Brick Description: A 78% alumina, bauxite based, quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from s.. |
|||
Maximum Service Temperature, Air | 1525 °C | 2777 °F | |
Gouda Vuurvast AK 80 AP Dense Refractory Brick Description: This phosphate bonded bauxite brick has an improved resistance against slag attack.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.. |
|||
Maximum Service Temperature, Air | 1525 °C | 2777 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 80 AP Dense Refractory Brick Description: This phosphate bonded bauxite brick has an improved resistance against slag attack.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.. |
|||
Maximum Service Temperature, Air | 1525 °C | 2777 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 82 A Dense Refractory Brick Description: A high alumina bauxite based quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from sa.. |
|||
Maximum Service Temperature, Air | 1525 °C | 2777 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast LP 80 A Dense Refractory Brick Description: LP 80 is a low porosity brick based on sintered bauxite with an extremely high abrasion resistance and therefore very well suited for application in rotary cement furnaces.Remarks: This.. |
|||
Maximum Service Temperature, Air | 1525 °C | 2777 °F | |
Gouda Vuurvast LP 80 A Dense Refractory Brick Description: LP 80 is a low porosity brick based on sintered bauxite with an extremely high abrasion resistance and therefore very well suited for application in rotary cement furnaces.Remarks: This.. |