Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Constant use; SAE J-2236 |
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Continuous; 20,000 h |
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data) This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Parker Chomerics SOFT-SHIELD® 5000 Low Closure Force EMI Gasket Description: SOFT-SHIELD® 5000 Series EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electron.. |
|||
Maximum Service Temperature, Air | <= 70.0 °C | <= 158 °F | |
Pearl Engineering PEPLPET B-105C PET Bottle Grade A co-polymer used for soft drinks and other applications. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Polycasa PETG QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits o.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Abatron 85071 A/B Filled Potting Compound
(discontinued **) High grade self leveling buff coating resufacer casting and adhesive resin. 100/20 ratio.Information provided by Abatron. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Maximum Service Temperature, Air | 70.0 - 93.3 °C | 158 - 200 °F | Average value: 75.1 °C Grade Count:14 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
GEHR Plastics ABS Acrylonitrile Butadiene Styrene Acrylonitrile Butadiene Styrene copolymer has a good thermal and dimensional stability and scratch resistance. Advantagesgood mechanical strengthresists scratchinghigh surface strengthhigh impact st.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
LATI Latiblend 5262 PP Homopolymer/PA6 Blend based on Polypropylene homopolymer (PPh) / Polyamide 6 (PA6). Unfilled. High impact resistance. Very good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Continuous Use |
Polyram PlusTek PA830 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Trelleborg R409 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Trelleborg R608 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Continuous Use |
Polyram PlusTek PB350M4 Nylon 6, 20% Mineral Filled 20% mineral filled polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Continuous Use |
Polyram PlusTek RA124 Nylon 6.6, Injection Molding Fast cycle polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Wet Service |
Chesterton ARC 982 100% Novolac acid resistant coating Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
ChevronTexaco Dura-Lith® NLGI 000 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | ASTM D 3575 |
Eurofoam Polycell PE 30 Polyethylene Foam Closed-cell polyethylene foam. Extruded reticulated pieces. Excellent physical properties both for active and static uses. Adjustable softness, elasticity, thermal deformation, shock absorbing. Use.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Deflection temperature; load unknown. |
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Long Term |
3M 4496W Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Maximum Service Temperature, Air | 70.0 - 80.0 °C | 158 - 176 °F | Average value: 75.6 °C Grade Count:8 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Constant use |
Saint-Gobain Lo-Skid® LS7000/LS7100 Series High Density Bumper and Footpad Urethane Foam Description: Lo-Skid™ LS7000 and LS7100 (acrylic adhesive on one side) urethane foam products are widely recommended for bumpers and footpads for applications and electronic products because it pro.. |
|||
Maximum Service Temperature, Air | 70.0 - 149 °C | 158 - 300 °F | Average value: 99.5 °C Grade Count:57 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |