Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Peak |
Pyrotek Dense Fused Silica Pre-Cast Shapes Pyrocast Dense Fused Silica is an economical product for shapes demanding thermal shock resistance at temperatures. Pyrocast DFS stands up to repeated use in molten metal casting in aluminum, coppe.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Continuous |
Pyrotek SF-50 Foamed Fused Silica Insulation Board SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 60 M Dense Refractory Brick Description: This quality is produced from high fired raw materials with a high mullite content. The grain distribution for these bricks is carefully selected, so that a maximum density is obtained... |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast CURAS 85 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This phosphate bonded material based on corundum and bauxite has a very go.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast LP 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. The extremely low porosity results in a very good slag resistance, a good abrasion resistance and high.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Sharadaa Ceramics HA 90SD High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Quick Immersion |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Intermittent |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Refractory Composites RS-99R Refractory Sheet Type RS-99R boards are prefired and are unaffected by moisture. They stay rigid even if saturated with water.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI) |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Cotronics Resbond™ 906 High Temperature Ceramic Adhesive, High Expansion |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Cotronics Resbond™ 908 High Temperature Ceramic Adhesive, Moisture Proof |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Cotronics Resbond™ 989 High Temperature, High Purity Alumina Adhesive, General Purpose |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories HACT-165G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories PTC-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories TCH-175S Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Anderman Ceramics EZZ 66P Zircon Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabind™ 643-1 High Temperature Inorganic Binder A basic solution compatible with most ceramic and metal powders. Excellent binder for producing high temperature protective coatings and refractory and chemically resistant adhesives and patching ma.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 569 High Temperature Ceramic Adhesive/Paste, Alumina Filled White paste used for bonding of Ceramic-to-Ceramic; Ceramic-Metal; and Quartz. Used in Heaters, Igniters, Resistors, Sensors. This one component system air dries in 1-2 hrs and is ready for use fol.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Continuous |
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Pyrotek Pyrocast AL2 Abrasion-Resistant Refractory Castable Pyrocast AL2 refractory castable is a mullite-based refractory well suited for applications prone to erosion and abrasion. It exhibits excellent non-wetting properties when used in molten aluminum .. |