Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 125 °C | 257 °F | Recommended |
Nye Lubricants 368F (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Recommended |
Nye Lubricants 723K (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Recommended |
Nye Lubricants 760A (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Recommended |
Nye Lubricants 868L (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Parker Chomerics Waveguide Gaskets 877 Conductive Silicone Elastomer Gasket Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Mechanical |
CE Phenolic Laminate Cotton based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many s.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Humiseal 1A27 Urethane Conformal Coating Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Humiseal 1A33LSE Urethane Conformal Coating Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Ball Pressure Temperature; IEC 60695-10-2 |
Mitsubishi Xantar® 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Ball Pressure Temperature; IEC 60695-10-2 |
Mitsubishi Xantar® MX 1071 FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Ball Pressure Temperature; IEC 60695-10-2 |
Mitsubishi Xantar® F 23 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Continuous |
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Tra-Con Tra-Bond 2222 One-Part Surface Mount Epoxy Adhesive TRA-BOND 2222 is a solvent-free, one-part thixotropic, epoxy adhesive recommended for SMD (Surface Mount Device) bonding and sealing applications where its easy handling, high strength and superior .. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Tra-Con Tra-Bond 2103 Medium Viscosity/Low Vapor Pressure Epoxy Adhesive TRA-BOND 2103 is a clear, near transparent, medium viscosity epoxy adhesive formulation developed for rigid laminating, sealing and bonding applications where the combination of good wetting plus im.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
ELASTO UK Dryflex® 502800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
ELASTO UK Dryflex® 502850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
ELASTO UK Dryflex® 600900S SEBS Based Material, Filled Qualities, 90A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
ELASTO UK Dryflex® 660500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
ELASTO UK Dryflex® 662450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Service |
3M FM07N Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Matte Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester ov.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Service |
3M FM142 Indoor UL Recognized Computer Imprintable Clear Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Service |
3M FM232 Indoor UL Recognized Matte Clear Polyester Label Products 3M™ Indoor UL Recognized Matte Clear Polyester Label Products FM23N, FM232 and FM239 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These po.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | Service |
3M 7031 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | at 50% loss of tensile strength after 20000h; IEC 216-1 |
BASF Ultradur® B 4406 G6 30% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Parker Chomerics CHO-SEAL 1215 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
Parker Chomerics CHO-SEAL 1217 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |
|||
Maximum Service Temperature, Air | 125 °C | 257 °F | |
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |