Polymer Property : Maximum Service Temperature, Air = 590 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 310 °C
590 °F
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer
Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur..
Maximum Service Temperature, Air 310 °C
590 °F
Precision Polymer Engineering Perlast® G60T Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: This grade is particularly suited to static ap..
Maximum Service Temperature, Air 310 °C
590 °F
Precision Polymer Engineering Perlast® G70H Perfluoroelastomer
Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p..
Maximum Service Temperature, Air 310 °C
590 °F
Precision Polymer Engineering Perlast® G70T Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter..
Maximum Service Temperature, Air 310 °C
590 °F
Precision Polymer Engineering Perlast® G80H Perfluoroelastomer
Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p..
Maximum Service Temperature, Air 310 °C
590 °F
Precision Polymer Engineering Perlast® G80T Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter..
Maximum Service Temperature, Air 310 °C
590 °F
Precision Polymer Engineering Perlast® G81H Perfluoroelastomer
Special, pure white compound with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. ..
Maximum Service Temperature, Air 310 °C
590 °F
Precision Polymer Engineering Perlast® G81T Perfluoroelastomer
A special black perfluoroelastomer compound with PTFE blended for improved mechanical performance. Excellent steam resistance and mechanical properties. Extremely low outgassing properties. Applica..
Maximum Service Temperature, Air 310 °C
590 °F
Short Periods
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet)
KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. ..
Maximum Service Temperature, Air 310 °C
590 °F
Precision Polymer Engineering Perlast® G71H Perfluoroelastomer
Special, white compound, with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. Appl..
Maximum Service Temperature, Air 310 °C
590 °F
Precision Polymer Engineering Perlast® G75S Perfluoroelastomer
Perlast® G75S has been specifically developed to cope with a wide range of process media, potent active pharmaceutical ingredients (APIs) and aggressive cleaning agents, being especially suited to ..
Maximum Service Temperature, Air 310 °C
590 °F
Continuous
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data)
Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic..
Maximum Service Temperature, Air 310 °C
590 °F
Short Periods
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet)
KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re..
Maximum Service Temperature, Air 310 °C
590 °F
DuPont Test Method
DuPont Performance Polymers Kalrez® 9500 Fluoroelastomer
DuPont™ Kalrez® 9500 perfluoroelastomer parts are a tan product for Deposition, Ash/Strip and Conductor (Poly/Metal) Etch processes. It has been specifically designed for use in applications where..
Maximum Service Temperature, Air 310 °C
590 °F
Short term
CENTROPLAST CENTROPEEK Polyetheretherketone
This plastic has high temperature resistance, good chemical resistance, and good mechanical characteristics. Its has good sliding friction properties and is suitable for use with foodstuffs or medi..