Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 316 °C | 600 °F | Intermittent |
Plasma Coatings 200-HT Surface Material Information provided by Plasma Coatings |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Intermittent |
Dielectric Polymers NT-590DL Protective Film
(discontinued **) Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized Class 392°FHigh temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications:.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Intermittent |
Dielectric Polymers NT-590 Polyimide Film Tape
(discontinued **) Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized class 392°FHigh temperature resistantClean tape removalApplications: For high temperature masking, protecting gol.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |
|||
Maximum Service Temperature, Air | >= 316 °C | >= 600 °F | |
Lubriplate 68 SYN High Temp 100% Ester-Based Multi-Purpose Synthetic Fluid These 100% ester-based synthetic lubricants are recommended for applications that are exposed to high operating temperatures and must maintain a clean lubricated surface. Available in ISO viscosity .. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvacore® A38T Flux Cored Brazing Alloy Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy Silvaloy 45 is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining s.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A38T Brazing Alloy Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A40T Brazing Alloy Silvaloy A40T is a good general purpose, low melting, cadmium-free alloy, often selected for its low temperature, wetting and good flow. Silvaloy A40T has a lower brazing temperature with a relative.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A45 Flux Coated Rod Brazing Alloy Silvaloy A45 FC is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is also used for brazing in electrical industry and for brazing b.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manu.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Greene Tweed CHEMRAZ® 551 Perfluoroelastomer With its broad chemical resistance, Chemraz® 551 is ideally suited as a universal sealing material for aqueous semiconductor wafer processing and chemical/DI water distribution systems. Chemraz .. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvacap 35490 Brazing Alloy Silvacap is a low brazing temperature, cadmium-free alloy. It has a slight plastic range which may be noticed during melting on some applications. Generally, the joint strength using Silvacap will s.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® 25 Brazing Alloy Silvaloy 25 is historically a modification of Silvaloy 30 with a further reduction in silver content resulting in a higher melting point and a longer melting range. Silvaloy 25 is used for brazing s.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® 50N Brazing Alloy Silvaloy 50N is a modification of Silvaloy 50. It was originally introduced because of somewhat better corrosion resistance than Silvaloy 50 for certain conditions, and is still used for such purpos.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | UL-746 B |
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Short Term |
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec.. |
|||
Maximum Service Temperature, Air | >= 316 °C | >= 600 °F | UL-746 B |
Saint-Gobain Meldin® 2211 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Ser.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Master Bond Mastersil 801 One Component, Room Temperature Curing, Silicone System MasterSil 801 is an easy to use, one component, high performance silicone elastomer compound. MasterSil 801 features non-corrosive cure and serviceability up to 300°C; it exhibits good stability at.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
W. L. Gore GORE™ 800 PTFE Universal Pipe Gasket (Style 800) 100% expanded PTFE, with multi-directional strength. Resistant to all media in the 0-14 pH range, except molten alkali metals and element fluorine, particularly at elevated temperatures and pressure.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Cotronics Duralco™ 133 500°F (260°C) Aluminum Filled Epoxy Two component, heat curing, aluminum filled epoxy suitable for high temperature tooling and a readily machinable repair or construction material. Similar to Duralco™ 132, but with a maximum servic.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Cotronics Duralco™ 4460 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant Excellent adhesion to metals, plastics, ceramics and glass. High bond strength, low moisture absorption, high thermal stability, low shrinkage and excellent chemical, electrical, and radiation resi.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Cotronics 4700 Ultra Temp Adhesive and Casting Epoxy, General Purpose |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Maximum Service Temperature, Air | >= 316 °C | >= 600 °F | UL-746 B |
Saint-Gobain Meldin® 2001 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |
|||
Maximum Service Temperature, Air | >= 316 °C | >= 600 °F | UL-746 B |
Saint-Gobain Meldin® 2030 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |