Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CQX10030E10 Polypropylene, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP EQX10030R UV Polypropylene, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T1030 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T1035 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC T15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC T5040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC T8040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB SCANTEC PC S85R Polycarbonate Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T10030 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH Q15030 E10 Polypropylene Homopolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 0.999 kg |
291 °F @Load 2.20 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND PSA 7400 HF PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendHigh impact resistance, high gloss, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 144 °C @Load 5.00 kg |
291 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTACARB 0820 GF Polycarbonate, 10% Glass Filled Polycarbonate with 10% glass fiber reinforcementHigh stiffness, good impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 144 °C @Load 5.00 kg |
291 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTACARB 1001 Polycarbonate General purpose polycarbonateHigh impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 144 °C @Load 5.00 kg |
291 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTACARB 1601 Polycarbonate General purpose polycarbonateHigh melt flow rate, high impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® FU1007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® FU4007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Vicat Softening Point | 144 °C @Load 5.10 kg |
291 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® LQ2647 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g.. |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH TS15010 H VTUV1 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC K8040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 144 °C @Load 1.00 kg |
291 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC T8020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |