Thermal Conductivity 1.82 - 1.92 W/m-K

@Temperature 100 °C
12.6 - 13.3 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 150 G RAPID Dense Vibrating Refractory Castable
Description: Vibron 150 G Rapid is a low cement castable based on sintered South-American bauxite. Because of special additives this material is suited for direct contact with liquid aluminum and al..
Thermal Conductivity 1.82 - 1.92 W/m-K

@Temperature 600 °C
12.6 - 13.3 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 150 G RAPID Dense Vibrating Refractory Castable
Description: Vibron 150 G Rapid is a low cement castable based on sintered South-American bauxite. Because of special additives this material is suited for direct contact with liquid aluminum and al..