Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.70 W/m-K @Temperature 1100 °C |
18.7 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 94 M Dense Refractory Brick Description: This mullite bonded, corundum brick combines a very good thermal shock resistance with a low creep as well as with resistance against a large variety of slags. (after 50 hours at 1650Â.. |
|||
Thermal Conductivity | 2.70 W/m-K @Temperature 100 °C |
18.7 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast LP 80 A Dense Refractory Brick Description: LP 80 is a low porosity brick based on sintered bauxite with an extremely high abrasion resistance and therefore very well suited for application in rotary cement furnaces.Remarks: This.. |