Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 183 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 26.3 W/m-K

@Temperature 23.0 °C
183 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications
Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st..
Thermal Conductivity 26.3 W/m-K

@Temperature 150 °C,
Time 3600 sec
183 BTU-in/hr-ft²-°F

@Temperature 302 °F,
Time 1.00 hour
+200°C/1 hr
Epoxy Technology EPO-TEK® EK1000 Epoxy
Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding ..
Thermal Conductivity 26.3 W/m-K

@Temperature 150 °C,
Time 3600 sec
183 BTU-in/hr-ft²-°F

@Temperature 302 °F,
Time 1.00 hour
+200°C/1 hr
Epoxy Technology EPO-TEK® EK1000-MP Epoxy
Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding ..
Thermal Conductivity 26.3 W/m-K

@Temperature 150 °C,
Time 3600 sec
183 BTU-in/hr-ft²-°F

@Temperature 302 °F,
Time 1.00 hour
+200°C/1 hr
Epoxy Technology EPO-TEK® EK2000 Epoxy
Preliminary Product Information SheetMaterial Description: A two component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance ..
Thermal Conductivity 26.3 W/m-K

@Temperature 500 °C
183 BTU-in/hr-ft²-°F

@Temperature 932 °F
Bohler-Uddeholm BÖHLER K294 MICROCLEAN AISI A11 Powder Metal Tool Steel
Properties: Powder-metallurgical produced cold work tool steel with extremely high wear resistance, good toughness and high compressive strength. The latest generation of powder metal technology ena..
Thermal Conductivity 26.4 W/m-K

@Temperature 100 °C
183 BTU-in/hr-ft²-°F

@Temperature 212 °F
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel
VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili..
Thermal Conductivity 26.3 W/m-K

@Temperature 500 °C
183 BTU-in/hr-ft²-°F

@Temperature 932 °F
AK Steel 430 Ferritic Stainless steel
AK Steel 430 combines good corrosion resistance and heat and oxidation resistance up to 1500°F with good mechanical properties. Typical consumer applications include automotive trim and molding, f..
Thermal Conductivity 26.3 W/m-K

@Temperature 500 °C
183 BTU-in/hr-ft²-°F

@Temperature 932 °F
AK Steel 430 ULTRA FORM® Stainless Steel
430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste..
Thermal Conductivity 26.3 W/m-K

@Temperature 500 °C
183 BTU-in/hr-ft²-°F

@Temperature 932 °F
AK Steel 434 Ferritic Stainless steel
AK Steel 434 is a modification of Type 430, the addition of molybdenum increases this alloy's corrosion resistance and its attack from many deicing chemicals. It also provides good heat and oxidati..
Thermal Conductivity 26.4 W/m-K

@Temperature 870 °C
183 BTU-in/hr-ft²-°F

@Temperature 1600 °F
Haynes 617 Nickel Alloy Plate
Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed..
Copyright © lookpolymers.com All Rights Reserved