Polymer Property : Thermal Conductivity = 24.4 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 24.4 W/m-K

@Temperature 500 °C
169 BTU-in/hr-ft²-°F

@Temperature 932 °F
International Mold Steel Daido DRM3 Matrix High-Speed Steel
This conventional grade MH88 has been improved to DRM3. High hardness and tough DRM3 with excellent hardenability is suitable for high precision cold working tools.Information provided by Internatio..
Thermal Conductivity 24.4 W/m-K

@Temperature 500 °C
169 BTU-in/hr-ft²-°F

@Temperature 932 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Annealed
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 24.4 W/m-K

@Temperature 500 °C
169 BTU-in/hr-ft²-°F

@Temperature 932 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 24.4 W/m-K

@Temperature 500 °C
169 BTU-in/hr-ft²-°F

@Temperature 932 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 24.4 W/m-K

@Temperature 500 °C
169 BTU-in/hr-ft²-°F

@Temperature 932 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 24.4 W/m-K

@Temperature 500 °C
169 BTU-in/hr-ft²-°F

@Temperature 932 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 24.4 W/m-K

@Temperature 500 °C
169 BTU-in/hr-ft²-°F

@Temperature 932 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 24.4 W/m-K

@Temperature 300 °C
169 BTU-in/hr-ft²-°F

@Temperature 572 °F
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel
Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr..
Thermal Conductivity 24.4 W/m-K

@Temperature 350 °C
169 BTU-in/hr-ft²-°F

@Temperature 662 °F
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel
Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr..