Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 26.4 W/m-K @Temperature 100 °C |
183 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili.. |
|||
Thermal Conductivity | 26.4 W/m-K @Temperature 870 °C |
183 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |