Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 382 °C | 720 °F | |
Indium Corp. Indalloy 176 Zinc Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 382 °C | 720 °F | Melting Point |
Lucas-Milhaupt AL 802 Aluminum Brazing Filler Metal Characteristics:AL 802 is a general purpose free flowing soldering filler metals for use with all solderable aluminum and aluminum alloys when soldering with torch. Information provided by Lucas-Mi.. |