Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -40.0 - 150 °C |
8.33 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 150 °C |
8.33 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -40.0 - 150 °C |
8.33 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 150 °C |
8.33 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -40.0 - 150 °C |
8.33 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 150 °C |
8.33 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 150 °C |
8.33 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -40.0 - 150 °C |
8.33 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM SF2350 PEI Blend High flow Ultem blends for thin wall application |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -40.0 - 150 °C |
8.33 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem SF2350 PEI Blend (Europe-Africa-Middle East) High flow Ultem blends for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -40.0 - 150 °C |
8.33 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM SF2360 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2; ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-4-280NA Polyphenylene Sulfide (PPS), Glass Fiber Ryton® R-4-280NA 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2; ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-7-190BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
2; ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2; ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
8.33 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DEL22P PC (Asia Pacific) LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
8.33 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU2410 PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
8.33 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |