Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 160 - 249 °C |
11.1 µin/in-°F @Temperature 320 - 480 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 0.000 - 100 °C |
11.1 µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 0.000 - 100 °C |
11.1 µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature >=143 °C |
11.1 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature <=143 °C |
11.1 µin/in-°F @Temperature <=289 °F |
Below Tg; ISO 11359 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature <=143 °C |
11.1 µin/in-°F @Temperature <=289 °F |
Below Tg; ASTM D696 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature <=143 °C |
11.1 µin/in-°F @Temperature <=289 °F |
Below Tg; ISO 11359 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature <=152 °C |
11.1 µin/in-°F @Temperature <=306 °F |
Below Tg; ISO 11359 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -20.0 - 150 °C |
11.1 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2300F PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 150 °C |
11.1 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2300F PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 100 - 200 °C |
11.1 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Amodel® A-1133 L WH 015 Polyphthalamide (PPA), 33% Glass Fiber Formerly referred to as Amodel® PXM-13015. Amodel® A-1133 L resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade featu.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 0.000 - 100 °C |
11.1 µin/in-°F @Temperature 32.0 - 212 °F |
2 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 0.000 - 100 °C |
11.1 µin/in-°F @Temperature 32.0 - 212 °F |
2 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 0.000 - 100 °C |
11.1 µin/in-°F @Temperature 32.0 - 212 °F |
2 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 0.000 - 100 °C |
11.1 µin/in-°F @Temperature 32.0 - 212 °F |
2 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 0.000 - 90.0 °C |
11.1 µin/in-°F @Temperature 32.0 - 194 °F |
2 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
11.1 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
11.1 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® R-4-240BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
11.1 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
11.1 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® XE4050BL Polyphenylene Sulfide Alloy (PPS Alloy), GlassMineral Filled Ryton® XE4050BL glass fiber and mineral filled polyphenylene sulfide alloy compound provides high ductility and impact strength along with good thermal stability.Features: Ductile; Good Thermal S.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
11.1 µin/in-°F @Temperature -58.0 - 122 °F |
2 |
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -40.0 - 150 °C |
11.1 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 0.000 - 100 °C |
11.1 µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature >=143 °C |
11.1 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |