Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4850 PBT+PC
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU
LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber.
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK
LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific)
LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 75-1/-2
BASF Ultrason® E 2010 MR SW 10111 PESU
Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 75-1/-2
BASF Ultrason® E 3010 MR UN PESU
Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat..
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 75-1/-2
BASF Ultrason® E 2010 HC PESU
Information provided by BASF
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 75-1/-2
BASF Ultrason® E 2010 SW Q31 10088 PESU
Information provided by BASF
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Asia Pacific)
LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber.