Polymer Property : CTE, linear, Parallel to Flow = 42.2 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® OQ3820 PC
High Viscosity, UV-stabilized grade for ophthalmic lenses.
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® OQ3820 PC (Asia Pacific)
High Viscosity, UV-stabilized grade for ophthalmic lenses.
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® OQ3820 PC (Europe-Africa-Middle East)
High Viscosity, UV-stabilized grade for ophthalmic lenses.
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific)
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 310SE0 PBT
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® HX215HP PBT
High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta..
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® HX215HP PBT
High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta..
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® HX3061HP PBT
PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only.
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® HX3061HP PBT
PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only.
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66
LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific)
LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized.
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA
Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to ..
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East)
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..