Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1010A PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1010A PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1010K PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.6 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1010P PEI Enhanced flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1100V PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1100V PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU1000E PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM HU1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 Conductive GTX, CTE 7 |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Asia Pacific) Conductive GTX, CTE 7 |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. US FDA and EU Food Contact compliant. |
|||
CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
30.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 75-1/-2 |
BASF Ultrason® P 3010 MR SW 10101 PPSU Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati.. |